Hoʻolako i ka Indium Oxide In2O3 ke kumukūʻai pauka me ka nui micron a me ka nui nano

ʻO ka wehewehe pōkole:

Ke Ana Hoʻohālike In2O3.20 In2O3.50
Nui ʻāpana 10-30nm 30-60nm
Poe Poʻo Poʻo
Maʻemaʻe(%) 99.9 99.9
ʻAnoʻulaʻula Melemele Pada Māmā Melemele Pada
BET(m2/g) 20~30 15~25
ʻOi aku ka nui (g/cm3) 1.05 0.4~0.7


Huahana Huahana

Huahana Huahana

Hōʻike huahana

INdex Model In2O3.20 In2O3.50
Nui ʻāpana 10-30nm 30-60nm
Kinohi pōʻai pōʻai
Maʻemaʻe(%) 99.9 99.9
ʻO ke ʻano Pauda Melemele Māmā Pauda Melemele Māmā
BET(m2/g) 20-30 15~25
ʻOi aku ka nui (g/cm3) 1.05 0.4-0.7
Hoʻopili: 1kg/ʻeke
  E mālama ʻia i loko o kahi kūlana i hoʻopaʻa ʻia, maloʻo a maloʻo, ʻaʻole e hōʻike i ka ea no ka manawa lōʻihi, e pale aku i ka makū.
Nā hiʻohiʻona: ʻO ka Indium oxide, ka indium hydroxide he mea hou n-type transparent semiconductor functional material, nona ka pūʻulu ākea ākea, kahi resistivity liʻiliʻi a me kahi hana catalytic kiʻekiʻe.palapala noi.Ma waho aʻe o nā hana i luna, hiki i ka nui o ka indium oxide i ke kiʻekiʻe nanometer, a me ka hopena o ka honua, ka hopena nui, ka hopena liʻiliʻi, a me ka hopena macro quantum tunnel o nā nanomaterials.
Noi: ʻO nā mea hoʻohui no nā pale fluorescent, aniani, seramika, kemika reagents, haʻahaʻa-mercury a me ka mercury-free alkaline batteries.Me ka hoʻomau mau ʻana o ka ʻepekema a me ka ʻenehana, ʻo ka hoʻohana ʻana i ka indium trioxide i loko o nā hōʻike aniani wai, ʻoi aku ka nui o nā pahuhopu ITO, e ulu ākea a ākea.
MEA OLELO HOOLAHA TXLT RXLULTS
Ka nana aku Pauda Melemele Malamalama Pauda Melemele Malamalama
In2O3(%,Min) 99.99 99.995
Nā haumia(%, Max)
Cu   0.8
Pb   2.0
Zn   0.5
Cd   1.0
Fe   3.0
Tl   1.0
Sn   3.0
As   0.3
Al   0.5
Mg   0.5
Ti   1.0
Sb   0.1
Co   0.1
K   0.3
Papa kuhikuhi 'ē aʻe
Ka nui o ka ʻāpana (D50)   3-5μm