Modèl | DK417 | DK417-3 | DK417-5 | DK417-8 | Crystal faz | Faz monoklinik | 3Y faz tetragonal | 5Y faz tetragonal | 8YKibik faz | ZrO2% (+ HfO2) | 99.9 | 94.7 | 91.5 | 86.5 | Y2O3(wt%) | - | 5.3±0.3 | 8.5±0.3 | 13.5±0.3 | Al2O3% ≤ | 0.005 | 0.01 | 0.01 | 0.01 | SiO2% ≤ | 0.005 | 0.01 | 0.01 | 0.01 | Fe2O3% ≤ | 0.003 | 0.01 | 0.01 | 0.01 | CaO% ≤ | 0.003 | 0.005 | 0.005 | 0.005 | MgO% ≤ | 0.003 | 0.005 | 0.005 | 0.005 | TiO2%≤ | 0.001 | 0.002 | 0.002 | 0.002 | Na2O% ≤ | 0.001 | 0.005 | 0.01 | 0.01 | Cl- % ≤ | 0.1 | 0.1 | 0.1 | 0.1 | Boule % ≤ | 0.8 | 0.8 | 0.9 | 0.85 | Gwosè an mwayèn patikil | 20nm | 20nm | 20nm | 20nm | Ranje aplikasyon: 1. Batri Aditif: Estabilize nano-zirkonya kòm yon elektwolit ideyal yo te lajman itilize nan selil gaz solid oksid. 2. Seramik fonksyonèl, seramik estriktirèl: seramik elektwonik, byoseramik, seramik Capteur, materyèl mayetik, elatriye;nano-zirkonya amelyore severite, fini sifas ak dansite seramik nan pati estriktirèl seramik. 3. Flite kouch, eleman piezoelectric, rezistans oksijèn sansib, kondansateur gwo kapasite. 4. Pyèr atifisyèl, materyèl abrazif, materyèl polisaj.Materyèl kouch fonksyonèl: ajoute nan kouch la gen anti-korozyon, efè anti-bakteri, amelyore rezistans mete. 5. Nano-zirkonya yo itilize pou materyèl refractory: elektwonik seramik boule sipò pad, fusion vè, metaliji metal refractory. |