Umzekelo | DK417 | DK417-3 | DK417-5 | DK417-8 | Isigaba seCrystal | Isigaba se-Monoclinic | Isigaba se-3Y se-tetragonal | Isigaba se-5Y se-tetragonal | 8YCubic isigaba | I-ZrO2% (+ HfO2) | 99.9 | 94.7 | 91.5 | 86.5 | Y2O3 (wt%) | - | 5.3±0.3 | 8.5±0.3 | 13.5±0.3 | Al2O3% ≤ | 0.005 | 0.01 | 0.01 | 0.01 | SiO2%≤ | 0.005 | 0.01 | 0.01 | 0.01 | Fe2O3%≤ | 0.003 | 0.01 | 0.01 | 0.01 | CaO%≤ | 0.003 | 0.005 | 0.005 | 0.005 | MgO%≤ | 0.003 | 0.005 | 0.005 | 0.005 | I-TiO2%≤ | 0.001 | 0.002 | 0.002 | 0.002 | Na2O%≤ | 0.001 | 0.005 | 0.01 | 0.01 | Cl- %≤ | 0.1 | 0.1 | 0.1 | 0.1 | Ukutshisa %≤ | 0.8 | 0.8 | 0.9 | 0.85 | Umyinge wobungakanani bamasuntswana | 20nm | 20nm | 20nm | 20nm | Uluhlu lwesicelo: 1. Izongezo zeBattery: Ukuzinzisa i-nano-zirconia njenge-electrolyte efanelekileyo isetyenziswe ngokubanzi kwiiseli eziqinileyo ze-oxide. 2. Iiseramics ezisebenzayo, iiseramics zesakhiwo: iiseramics ze-elektroniki, i-bioceramics, i-sensor ceramics, imathiriyeli yamagnetic, njl.; I-nano-zirconia iphucula ukuqina, ukugqitywa komphezulu kunye nokuxinana kwe-ceramic ye-ceramic structural parts. 3. Ukutshiza ukutyabeka, i-piezoelectric element, i-oxygen sensitive resistor, i-capacitor umthamo omkhulu. 4. Amatye anqabileyo okwenziwa, izinto ezinqabileyo, izinto zokupholisa. Izinto zokugqoka ezisebenzayo: zongezwa kwi-coating ukuze ibe ne-anti-corrosion, i-anti-bacterial effect, iphucula ukuxhatshazwa kokugqoka. 5. I-Nano-zirconia isetyenziselwa izinto eziphikisayo: i-electronic ceramic burning support pad, iglasi edibeneyo, i-metallurgical metal refractory. |